    If you have not seen an SLS part, see if you can get a sample first. They tend to have a rough powdery look and feel to them, and are difficult to impossible to sand smooth. I will check in my office in the morning to see if I have a sample I can take a close up photo of. For texture and not to disclose any confidential features. If the somewhat rough/porous surface is not contrary to the look you are going for that it will be a good choice. If it is printed in a black and you put a matte or flat clear over it, it might give a fair resemblance of black cast iron.