    This is very informative, nice to know there are options that don't include using dangerous acids (I was so worried I'd accidentally spill it somehow and put myself in the ER).
    Will this work on a chrome-plated brass sink tube? I'm thinking of etching deep enough to actually let the brass show, which I think would be a very nice look. May make it too thin and weak, but I figure it's worth a try. It looks great in my head, ha ha.

  2. #32

    Default

    I've had that same thought but have not tried it. As such, I have no idea how well chrome will etch.

    http://s6.photobucket.com/albums/y23...0Saber%20Hilts

    From Wikipedia: "Internet Explorer slows down GIFs if the framerate is 20 frames per second or higher and Microsoft reports that Google Chrome and Safari also slow down some GIF animations."

  3. #33

    Default

    Well, I suppose I'll have to try it. Not like it's much of an investment to give it a trial run.