    Id be intrested to see the effect, personnely id just stick to 1 layer, especialy if you plan to have a sheath go over the top.
    Nearly all men can stand adversity, but if you want to test a man's character, give him power.

  2. #12

    Default

    I know Tim here at TCSS only does one colour per part at a time but I wonder if he'd do a two layered PC like you mention. Tim? lol

  3. #13
    Sith Minion mihunai's Avatar
    Join Date
    Mar 2009
    Location
    The Netherlands
    Posts
    449

    Default

    Doesnt the amount of layers it can hold, depend more on the individual properties of the layer's themselves?

    Especially max. temperatures.

    Lets say layer one cures at 230 degrees, and 'burns' at 290,
    whereas layer two cures at 300 degrees, and doesnt burn until 400 degrees.

    A situation like this means you cant use these two PC's.

    I mean, I'm no expert on powdercoating, let that be clear, but I can see a situation like this
    popping up in certain cases...

    mTm


    Official Owner of Skottsaber at Bowling

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •