Id be intrested to see the effect, personnely id just stick to 1 layer, especialy if you plan to have a sheath go over the top.
I know Tim here at TCSS only does one colour per part at a time but I wonder if he'd do a two layered PC like you mention. Tim? lol
Doesnt the amount of layers it can hold, depend more on the individual properties of the layer's themselves?
Especially max. temperatures.
Lets say layer one cures at 230 degrees, and 'burns' at 290,
whereas layer two cures at 300 degrees, and doesnt burn until 400 degrees.
A situation like this means you cant use these two PC's.
I mean, I'm no expert on powdercoating, let that be clear, but I can see a situation like this
popping up in certain cases...